Description:
Abstract. Research in PT Nusa Halmahera Minerals (NHM) is about gold and silver processing, especially for samples blending or parcel with composition in red kencana (KR-1873), yellow (TY2-214), mud kencana red mill (KR-1869). The purpose of this study is to determine the % recovery of gold (Au) and silver (Ag) with variations in cyanide (CN-) concentration and particle size. The result shows that the highest % recovery is reached at 35,3 micron size particles with 300 ppm cyanide (CN-) concentrations, where is able to extract gold (Au) of 92,77 % and silver (Ag) of 93,79%. This shows that in order to increase % recovery of gold (Au) and silver (Ag), the particle size and cyanide (CN-) concentration are one of the cyanide (CN-) leaching parameters that can extract more than other parameters.Keywords: Gold (Au) and Silver (Ag), Leaching, Particle Size, Cyanide (CN-) Concentration, Recovery. Abstrak. Penelitian di PT Nusa Halmahera Mineral (NHM) tentang pengolahan emas dan perak khususnya untuk sampel blending atau parcel dengan komposisi pada kencana red (KR-1873), kencana yellow (KY1-1163), toguraci yellow (TY2-214), mud (lumpur) mill kencana red (KR-1869). Tujuan penelitian ini adalah untuk mengetahui perolehan emas (Au) dan perak (Ag) dengan variasi konsentrasi sianida (CN-) dan variasi ukuran partikel. Berdasarkan hasil penelitian % perolehan tertinggi yaitu berada pada ukuran partikel 35.3 micron dengan konsentasi sianida (CN-) 300 ppm. Dimana mampu mengekstraksi emas (Au) sebesar 92.77% dan perak (Ag) sebebesar 93.79%. Hal ini menunjukan bahwa untuk meningkatkan % perolehan dari emas (Au) dan perak (Ag) maka parameter ukuran partikel dan konsentrasi sianida (CN-) merupakan salah satu parameter pelindian sianida (CN-) yang mampu mengekstraksi lebih banyak dari pada parameter lainnnya.Kata Kunci : Emas (Au) dan Perak (Ag), Pelindian, Ukuran Partikel, Konsentrasi Sianidasi (CN-), Perolehan.